From: Ultra-High Performance Concrete: Mechanical Performance, Durability, Sustainability and Implementation Challenges
References
w/b
Curing conditions
Fiber
Sorptivity coefficient (kg/m2/h0.5)
Roux et al. (1996)
0.14
20 °C water cured
2Â %
0.0100
0.0052
Franke et al. (2008)
0.17
90 °C for 2 days
No fiber
0.0330
0.19
0.0440