From: Enhancing Structural Resilience: Microbial-Based Self-Healing in High-Strength Concrete
No
Content
Batch weights (Kg/m3)
Ratio with cement
1
Cement
644.3
2
Fine aggregate
504.5
0.78
3
Coarse aggregate
1101.3
1.71
4
Water
200.4
0.3