From: Enhancing Structural Resilience: Microbial-Based Self-Healing in High-Strength Concrete
Concrete specimen made with | % Decrease as compared to the control (55% stress-level crack-initiated and healed specimen) | % Decrease as compared to the control (ordinary specimen) |
---|---|---|
S. koreensis | 2.6 | 4.3 |
B. flexus | 13.1 | 15.7 |