From: Shear Behavior and Performance of Deep Beams Made with Self-Compacting Concrete
SiO2 (%) | Al2O3 (%) | Fe2O3 (%) | CaO (%) | Na2O (%) | K2O (%) | MgO (%) | SO3 (%) | LOI | ρ (g/cm3) | SSA (cm2/g) | |
---|---|---|---|---|---|---|---|---|---|---|---|
OPC | 21.60 | 6.00 | 3.10 | 61.40 | – | – | 3.40 | 2.50 | 0.03 | 3.15 | 3,539 |
SG | 33.33 | 15.34 | 0.44 | 42.12 | – | – | 5.70 | 2.08 | 3.00 | 2.90 | 4,159 |
FA | 58.20 | 26.28 | 7.43 | 6.51 | 0.80 | – | 1.10 | 0.30 | 3.20 | 2.18 | 3,550 |