From: Study on Neutralization Progress Model of Concrete with Coating Finishing Materials in Outdoor Exposure Conditions Based on the Diffusion Reaction of Calcium Hydroxide
W/C (%)
S/A (%)
Unit amount (kg/m3)
Slump (mm)
Air content (%)
Compressive strength (N/mm2)
Water
Cement
Fine aggregate
Aggregate
60
47.9
176
271
862
952
180
4.5
29