Table 2 Repair mortar properties (provided by the manufacturer).

From: Rapid Repair of Severely Damaged RC Columns with Different Damage Conditions: An Experimental Study

Property

Results

Test Method

Fresh wet density, lb/ft3 (kg/m3)

142 (2,275)

ASTM C 138

Compressive strength, psi (MPa); 2 in. (51 mm) cubes

 

ASTM C 109

1 day

2,500 (17.2)

 

7 days

5,000 (34.5)

 

28 days

6,000 (41.4)

 

Compressive strength, psi (MPa); 3 by 6 in. (76 by 152 mm) cylinders, at 28 days

5,000 (34.5)

ASTM C 39

Flexural strength, psi (MPa), at 28 days

1,150 (7.9)

ASTM C 348

Slant shear bond strength, psi (MPa), at 28 days

3,000 (20.7)

ASTM C 882 (modified)

Splitting tensile strength, psi (MPa), at 28 days

500 (3.4)

ASTM C 496