From: Investigation of Likelihood of Cracking in Reinforced Concrete Bridge Decks
Manufacturer’s data | Lab test data (first attempt) | Lab test data (second attempt) | |||||
---|---|---|---|---|---|---|---|
Product | Tensile strength | Viscosity (cps) | Elongation (%) | Tensile strength | Elongation (%) | Tensile strength | Elongation (%) |
MPa | MPa | MPa | |||||
1-A | 56.4 | 5–15 | 5.5 | 22.6 | 2.1 | 25.3 | 2.6 |
2-B | 41.0–47.9 | 30 | 3–7 | 23.4 | 10.5 | 27.2 | N/A |
3-C | 19.3 | 5–20 | 40–50 | 0.9 | 99.6 | 7.3 | 17.2 |
4-D | 8.2 | 10–25 | 30 | No test | No test | 5.7 | 1.3 |
5-E | 6.9 | 80 | 60 | 3.3 | 213 | 5.4 | 102 |