Skip to main content

Table 2 Mix proportion by replacement and CRCA fabrication.

From: Characterization of Recycled Coarse Aggregate (RCA) via a Surface Coating Method

Type

Remarks

W/C = 49.9 %; S/a = 48.2 % (binder: 347 kg/m3) Superplasticizers = 0.5 % of cement wt%

Control (CCA 100 %) RCA 100 %

CRCA (25, 50, 75, and 100 %)

CRCA’s film

PC dispersant = ratio of 1 % of RCA’s wt%