Fig. 6From: Comparison of ASR Mitigation MethodologiesRIE of mortar bars prepared with two dosages of Class F fly (15 and 20 %) and lithium-to-alkali molar ratio of 0.74 (100 % Li) at various immersion ages. a RA-A aggregate. b RA-B aggregate. c RA-C aggregate. d RA-D aggregate.Back to article page