From: Comparison of ASR Mitigation Methodologies
Design Criteria
Portland cement (g)
Fly ash (g)
Lithium (g)
15 % FA + 100 % Li
872.7
154.0
47.23
20 % FA + 100 % Li
821.3
205.4