Table 1 Composition of SMCP.

From: Evaluation on the Mechanical Performance of Low-Quality Recycled Aggregate Through Interface Enhancement Between Cement Matrix and Coarse Aggregate by Surface Modification Technology

W/C (%)

W (mL)

C

Fe2O3 (%)

Volume (mL/L)

Weight (g/L)

30

487

513

1620

C × 100

  1. W water, C cement: density of cement: 3.16 g/cm3.