Table 1 Mix proportions of HRPC.

From: Tensile Properties of Hybrid Fiber-Reinforced Reactive Powder Concrete After Exposure to Elevated Temperatures

Series

Binding materials (kg/m3)

Quartz sand (kg/m3)

Water reducer (kg/m3)

Water (kg/m3)

Steel fiber (%)

PPF (%)

Cement

Silica fume

Slag

HRPC1

799.72

239.92

119.96

959.66

46.38

231.92

2

0.1

HRPC2

798.90

239.67

119.84

958.68

46.34

231.68

2

0.2

HRPC3

807.07

242.12

121.06

968.48

46.81

234.05

1

0.2

  1. Steel fibers and polypropylene fibers content are the volume dosage.