From: A Study on Residual Compression Behavior of Structural Fiber Reinforced Concrete Exposed to Moderate Temperature Using Digital Image Correlation
Material
Poly-propylene
Form
Structural fiber
Specific gravity
0.91
Length
60 mm
Tensile strength
618 N/mm2
Modulus of elasticity
10 GPa
Width
1.68 mm
Depth
0.60 mm
Melting temperature
180 °C
Decomposition temperature
360 °C