Table 7 Compressive strength of concrete samples at 28 days.

From: Temperature Reduction of Concrete Pavement Using Glass Bead Materials

Strength class

Glass bead proportion (% weight of aggregate)

Compressive strength (MPa)

C30/37

0

48.06

C30/37

9

42.48

C30/37

19

39.65

C30/37

31

35.57