Fig. 12From: Mechanical Properties and Modeling of Amorphous Metallic Fiber-Reinforced Concrete in CompressionCrack patterns of specimens with different fiber volume fractions (V f ) after failure: a V f = 0 %; b V f = 0.3 %; c V f = 0.6 %; and d V f = 0.8 %.Back to article page