Skip to main content

Table 3 Mix proportion (weight ratio).

From: Shear Tests for Ultra-High Performance Fiber Reinforced Concrete (UHPFRC) Beams with Shear Reinforcement

Water-binder ratio

Cement

Zirconium

Filler

Fine aggregate

Water-reducing admixture

0.2

1.0

0.25

0.3

1.1

0.02