From: Control of Tensile Behavior of Ultra-High Performance Concrete Through Artificial Flaws and Fiber Hybridization
Mixture ID
Density (g/cm3)
Measured
Theoretical
M-S
2.50 ± 0.02
2.44
M-S-PB
2.48 ± 0.02
2.42
M-PE
2.45 ± 0.03
2.41
M-PE-PB
2.40 ± 0.02
2.38