From: Pull-out Strengths of GFRP-Concrete Bond Exposed to Applied Environmental Conditions
Exposure duration (days)
Mean pull-out strength (MPa)
CoV of pull-out strength (%)
0
1027
6.0
35
1056
5.5
90
1065
1.9
365
1113
1.7