From: Pull-out Strengths of GFRP-Concrete Bond Exposed to Applied Environmental Conditions
Exposure duration (days)
Mean pull-out strength (MPa)
CoV of pull-out strength (%)
0
1027
6.0
28
1022
10.8
168
961
12.4
364
1011
6.9
546
1034
5.0