Skip to main content

Table 6 Pull-out strengths of GFRP outdoor environment specimens.

From: Pull-out Strengths of GFRP-Concrete Bond Exposed to Applied Environmental Conditions

Exposure duration (days)

Mean pull-out strength (MPa)

CoV of pull-out strength (%)

0

1027

6.0

60

941

7.0

180

931

6.3

365

970

7.0

555

1023

6.3