Table 1 Composition of componentsofcement samples.

From: Optimum Proportion of Masonry Chip Aggregate for Internally Cured Concrete

Component

Mass (%)

CaO

56.74

SiO2

22.83

Al2O3

8.66

Fe2O3

2.89

MgO

4.40

SO3

2.80

Na2O

0.10

K2O

0.73

TiO2

0.58

P2O5

0.13

MnO

0.05

Cr2O3

0.017

SrO

0.045

ZnO

0.008

Cl

0.000