Skip to main content

Table 4 Percent increase in modulus of elasticity with respect to control samples under similar curing conditions (w/c ratio 0.4).

From: Optimum Proportion of Masonry Chip Aggregate for Internally Cured Concrete

Percent replacement

Curing conditions

IC1

IC2

IC3

IC4

10

18

7.5

15

11

20

19.5

18.5

19.5

17

30

20

10

12.5

11