Fig. 5From: Strength Developments and Deformation Characteristics of MMA-Modified Vinyl Ester Polymer ConcreteCuring age versus compressive strength with curing temperature. a MMA 0 wt%, b MMA 2.5 wt%, and c MMA 5 wt%.Back to article page