Table 1 Mix proportions of concrete.

From: Maintenance for Repaired RC Column Exposed to Chloride Attack Based on Probability Distribution of Service Life

 

W/B (%)

S/a (%)

Unit weight (kg/m3)

SP (%)

W

C

SG

S

G

OPC

37

42.0

168

454

0

767

952

9.08

SG30

42

42.0

168

280

120

972

783

5.61

SG50

47

42.0

168

179

179

853

832

3.58