Skip to main content

Table 2 Results of steel tensile test.

From: Effects of Variation of Axial Load on Seismic Performance of Shear Deficient RC Exterior BCJs

Specimen Bar size (mm) Stress (MPa) Strain µε (Micro strain)
f y f u y u
SP1-SP7 Ø8 580 667 3000 10,500
Ø20 605 695 3100 10,600