Skip to main content

Table 1 Experimental plan.

From: Control of Viscosity of Cementitious Materials Using Waste Limestone Powder

Mixture conditions

Tests

Water-to-binder ratio

Available dosage of SP (% of binder weight)

Replacement ratio of WLP (% of cement weight)a

0.20

3.5, 4.0

0, 10, 20, 30

Powder conditions (Particle size distributions, specific surface, packing density)

Spread test

Plastic viscosity

0.25

0.8, 1.0, 1.2

0.30

0.5, 0.8

  1. a The replaced powder was prepared with three different levels of fineness.