From: Evaluation on Protection Performance and On-Site Applicability of Hybrid Fiber-Reinforced Concrete
Experimental conditionsa | Slump (mm) | Slump flow (mm) | Air content (%) |
---|---|---|---|
The first test | |||
 Before pumping | 130 | 225/220 | 4.0 |
 After pumping | 170 | 240/300 | 3.6 |
The second test | |||
 Before pumping | 135 | 230/240 | 3.8 |
 After pumping | 160 | 310/280 | 3.5 |