TYPE

Admixture (superplasticizer)

Cement

Silica fume

Water

Sand

Gravel

HPFRCC mortar ratio

0.14% bindera weight

1

0.1

0.28

1

–

Conventional concrete

–

1

–

0.45

1.72

1.72