Fig. 25From: Pullout Behaviour of Different Types of Steel Fibres Embedded in Magnesium Phosphate Cementitious MatrixEffect of fibre spacing on the average pullout energy up to 1.5 mm (H-2 fibre; specimens cured for 7 days).Back to article page