Table 4 Energy dissipation results

From: Flexural Strengthening of RC Columns with Low Longitudinal Steel Ratio using GFRP Bars

Specimen

Energy dissipation (kN m)

Increase in energy dissipation (%)

NS

7.71

–

S08

13.41

74

S10

17.19

122

S12

20.37

164