Skip to main content

Table 3 Stress levels of HRPC for STC testing.

From: Effects of Temperature and Stress on Creep Behavior of PP and Hybrid Fiber Reinforced Reactive Powder Concrete

Temperature ( °C)

Measured in MPa

\(f_{c}^{T}\)

20%

40%

60%

120

130.8

26.2

52.3

78.5

300

119.0

23.8

47.6

71.4

500

99.4

19.9

39.8

59.7

700

64.2

12.8

25.7

38.5

900

36.4

7.3

14.6

21.9