From: Effects of Temperature and Stress on Creep Behavior of PP and Hybrid Fiber Reinforced Reactive Powder Concrete
Strength ratios
Measured in MPa
HRPC
PRPC
\(f_{c}\)
151.1
97.0
10%
15.1
9.7
20%
30.2
19.4
30%
45.3
29.1
40%
60.4
38.8
50%
75.5
48.5
60%
90.6
58.2