No climate change | Water (kg/m3) | Cement (kg/m3) | Slag (kg/m3) | Fine aggregate (kg/m3) | Coarse aggregate (kg/m3) | Superplasticizer (kg/m3) |
---|---|---|---|---|---|---|
Mix1: design strength of 25Â MPa | 174.06 | 110.21 | 257.16 | 900.00 | 908.40 | 0.85 |
Mix2: design strength of 35Â MPa | 174.06 | 110.21 | 257.16 | 900.00 | 908.40 | 0.85 |
Mix3: design strength of 45Â MPa | 174.09 | 136.42 | 318.31 | 895.14 | 826.28 | 4.22 |
Mix4: design strength of 55Â MPa | 174.48 | 170.05 | 396.78 | 834.18 | 780.00 | 7.01 |