Climate change | Water (kg/m3) | Cement (kg/m3) | Slag (kg/m3) | Fine aggregate (kg/m3) | Coarse aggregate (kg/m3) | Superplasticizer (kg/m3) |
---|---|---|---|---|---|---|
Mix5: design strength of 25Â MPa | 174.04 | 121.04 | 282.43 | 900.00 | 872.07 | 2.42 |
Mix6: design strength of 35Â MPa | 174.04 | 121.04 | 282.43 | 900.00 | 872.07 | 2.42 |
Mix7: design strength of 45Â MPa | 174.09 | 136.42 | 318.31 | 895.14 | 826.28 | 4.22 |
Mix8: design strength of 55Â MPa | 174.48 | 170.05 | 396.78 | 834.18 | 780.00 | 7.01 |