Table 2 Identification of the concrete mixes.

From: Studies on Hemp and Recycled Aggregate Concrete

Mix no.

Mix ID

MSA (mm)

%Replacement of NCA by RCA

Fiber length (mm)

Fiber treatment

Group 1 MSA = 10 mm

 1

N10 (control 10)

10

0

 2

R10

10

50

 3

N10–H20–T1

10

0

20

Alkali

 4

R10–H20–T1

10

50

20

Alkali

 5

R10–H20–T2

10

50

20

Acetyl

 6

N10–H30–T1

10

0

30

Alkali

 7

R10–H30–T1

10

50

30

Alkali

Group 2 MSA = 20 mm

 8

N20 (control 20)

20

0

 9

R20

20

50

 10

N20–H20–T1

20

0

20

Alkali

 11

R20–H20–T1

20

50

20

Alkali

 12

N20–H20–T2

20

0

20

Acetyl

 13

R20–H20–T2

20

50

20

Acetyl

 14

N20–H30–T1

20

0

30

Alkali

 15

R20–H30–T1

20

50

30

Alkali

 16

R20–H30–T2

20

50

30

Acetyl