From: Investigation on the Mechanical Properties and Microstructure of Eco-friendly Mortar Containing WGP at Elevated Temperature
Mixes
Cement (g)
WGP (%)
WGP (g)
Sand (g)
W/C
Superplasticizer (%)
G0
500
0
1375
0.485
0.4
G5
475
5
25
0.3
G10
450
10
50
0.2
G15
425
15
75
0.1