Table 3 Mix proportion of cement pastes.

From: Characteristics of Wood Ash Cement Mortar Incorporating Green-Synthesized Nano-TiO2

Sample number

Sample designation

Weight of cement (g)

Weight of WA (g)

Weight of NT (g)

Weight of water (g)

Water/binder ratio

1

CEM 1 (control)

500

–

–

180

0.36

2

90CEM1 + 10WA

450

50

–

195

0.39

3

90CEM1 + 10WA + 1NT

450

50

5

187

0.37

4

90CEM1 + 10WA + 2NT

450

50

10

183

0.37

5

90CEM1 + 10WA + 3NT

450

50

15

181

0.36