From: Characteristics of Wood Ash Cement Mortar Incorporating Green-Synthesized Nano-TiO2
Sample code | Sample designation | Weight of cement (g) | Weight of WA (g) | Weight of SASS (g) | Weight of NT (g) | Weight of water (g) |
---|---|---|---|---|---|---|
A | CEM 1 + SASS (control) | 450 | – | 1350 | – | 225 |
B | 90CEM1 + 10WA + SASS | 405 | 45 | 1350 | – | 225 |
C | 90CEM1 + 10WA + 1NT + SASS | 405 | 45 | 1350 | 4.5 | 220.5 |
D | 90CEM1 + 10WA + 2NT + SASS | 405 | 45 | 1350 | 9.0 | 216 |
E | 90CEM1 + 10WA + 3NT + SASS | 405 | 45 | 1350 | 13.5 | 211.5 |