Table 5 Water absorption characteristics of WA cement mortar incorporating NT.

From: Characteristics of Wood Ash Cement Mortar Incorporating Green-Synthesized Nano-TiO2

Specimen identification

Weight before immersion (g)

Weight after immersion (g)

Weight of water absorbed (g)

Percentage of water absorbed (%)

Average (%)

K1

K2

K3

525.2

526.9

526.9

557.5

558.2

559.4

32.3

31.3

32.5

6.2

5.9

6.2

6.1

L1

L2

L3

515.3

518.5

513.0

551.4

554.4

548.1

35.8

35.9

35.1

6.9

6.9

6.8

6.8

M1

M2

M3

507.7

508.1

511.4

540.8

541.7

545.3

33.1

33.6

33.9

6.5

6.6

6.6

6.6

N1

N2

N3

517.7

519.7

516.1

547.8

551.5

547.6

30.1

31.8

31.5

5.8

6.1

6.1

6.0

O1

O2

O3

512.0

520.7

518.3

543.6

553.0

551.1

31.6

32.3

32.8

6.2

6.2

6.3

6.2

  1. KEY: K = CEM1 L = 90CEM1 + 10WA M = 90CEM1 + 10WA + 1NT
  2. N = 90CEM1 + 10WA + 2NT O = 90CEM1 + 10WA + 3NT