Fig. 4From: Study on the Fracture Toughness of Polypropylene–Basalt Fiber-Reinforced ConcretePartial production procedures of specimens: a aggregate drying; b stir aggregates; c scatter basalt fiber; d scatter polypropylene fiber; e table vibrator; f coating maintenance; g cutting and polishing; and h specimen sample.Back to article page