Table 4 Test results of HSSSWR-reinforced ECC specimens.

From: Tensile Behavior of High-Strength Stainless Steel Wire Rope (HSSSWR)-Reinforced ECC

Group number fse,cr(MPa) εse,cr(%) fse,u (MPa) εse,u (%) fws(MPa) εws(%) wmax,ws (mm) wmax,u(mm) Ese(MPa) TIp TIt
A1 2.20 0.0190 7.06 3.087 6.52 1.987 0.28 1.13 11,579 0.1670 0.1846
A2 2.25 0.0192 7.74 3.106 6.94 2.215 0.22 1.07 11,719 0.1875 0.2054
A3 2.41 0.0196 8.57 3.158 7.77 1.896 0.20 0.87 12,296 0.2075 0.2235
A4 2.56 0.0202 10.15 3.289 9.55 2.081 0.13 0.73 12,673 0.2462 0.2556
A5 2.44 0.0197 8.65 3.112 7.79 1.908 0.21 0.88 12,386 0.1893 0.2182