Rebar diameter (mm) Yield tensile strength (MPa) Ultimate tensile strength (MPa) Modulus of elasticity (GPa) Axial yield strain (mm/mm, %)
8 340 500 210 1.2 × 10–3
10 340 500 210 1.2 × 10–3