From: Study on Mechanical Properties of Polycaprolactone Modified Cement-Based Material
No. | Water (W) | Cement (C) | Standard sand (S) | PCL content/% | Water bath temperature/℃ | Water bath time/min | Curing time /d |
---|---|---|---|---|---|---|---|
2–1 | 0.6 | 1 | 3 | 0 | 70 | 30 | 28 |
2–2 | 0.6 | 1 | 3 | 1 | 70 | 30 | 28 |
2–3 | 0.6 | 1 | 3 | 2 | 70 | 30 | 28 |
2–4 | 0.6 | 1 | 3 | 3 | 70 | 30 | 28 |
2–5 | 0.6 | 1 | 3 | 5 | 70 | 30 | 28 |
2–6 | 0.6 | 1 | 3 | 10 | 70 | 30 | 28 |
2–7 | 0.6 | 1 | 3 | 15 | 70 | 30 | 28 |
2–8 | 0.6 | 1 | 3 | 20 | 70 | 30 | 28 |
2–9 | 0 | 0 | 1 | 60 | 70 | 30 | 28 |