From: Research on Modified High-Performance Cement Mortar of Prefabricated Buildings Based on Orthogonal Test
Solid content/(%)
Ash content at 600 ℃/(%)
Bulk density/(g/L)
Average particle size/
(μm)
Minimum film forming temperature /(℃)
98
13
450
80
6