Table 3 Fiber addition rate according to fiber type and manufacturer specifications (Nycon, 2019).

From: Study on Early-Age Elastic Modulus of FRC Using Electrical Resistivity and Resonance Frequency

Addition rate

Polypropylene

Nylon

Glass

Steel

Plastic shrinkage cracking

0.9 kg/m3

0.6 kg/m3

0.30–0.60 kg/m3

10–15 kg/m3

Performance of structure

N/A

N/A

5–15 kg/m3

15–80 kg/m3