Fig. 2From: Performance of CO2-Cured Alkali-Activated Slag Pastes During Curing and ExposureCompressive strength of alkali-activated slag subjected to CO2, measured at 3 days, and its preservation at 7 or 28 days after subsequent water bath (WB) curing and immersion in seawater (SW)Back to article page