From: Durability Properties and Microstructure of Ground Granulated Blast Furnace Slag Cement Concrete
Mix | w/c | a/c | GGBS (%) | Total cementitious materials (kg/m3) |
---|---|---|---|---|
C1 | 0.5 | 3 | 0 | 514 |
C2 | 0.5 | 4 | 0 | 424 |
C3 | 0.5 | 5 | 0 | 365 |
C4 | 0.4 | 3 | 0 | 526 |
C5 | 0.4 | 4 | 0 | 438 |
C6 | 0.6 | 4 | 0 | 407 |
G1 | 0.5 | 3 | 10 | 501 |
G2 | 0.5 | 3 | 30 | 498 |
G3 | 0.5 | 3 | 50 | 497 |
G4 | 0.5 | 4 | 50 | 418 |
G5 | 0.6 | 4 | 50 | 402 |
G6 | 0.4 | 4 | 50 | 436 |