Skip to main content

Table 2 Formulation code and the mix proportions of the components for the fabrication of the control cement mortar and ACM based mortar.

From: Investigation on the Effectiveness of Aqueous Carbonated Lime in Producing an Alternative Cementitious Material

Sample code

Mix proportioning of the components

Cement (g)

Fine aggregate (g)

Water (ml)

Alkali activator (ml)c

CCM

100a

300

60

ACM-M1

100b

300

60

ACM-M2

100b

300

30

30

ACM-M3

100b

300

60

  1. aOrdinary portland cement.
  2. bAlternative cementitious material.
  3. c50 % NaOH solution.