Fig. 11
From: Utilization of Waste Glass Micro-particles in Producing Self-Consolidating Concrete Mixtures

Flexural strength of SCC with GWG microparticles in different ages.
From: Utilization of Waste Glass Micro-particles in Producing Self-Consolidating Concrete Mixtures
Flexural strength of SCC with GWG microparticles in different ages.