Fig. 6
From: Utilization of Waste Glass Micro-particles in Producing Self-Consolidating Concrete Mixtures
![Fig. 6](http://media.springernature.com/full/springer-static/image/art%3A10.1007%2Fs40069-016-0141-z/MediaObjects/40069_2016_141_Fig6_HTML.gif)
Compressive strength of SCC with GWG microparticles as ages.
From: Utilization of Waste Glass Micro-particles in Producing Self-Consolidating Concrete Mixtures
Compressive strength of SCC with GWG microparticles as ages.